CuSn11Pb2-C / CuSn11Pb2-B, (CC482K)
Common name | Material description | World specifications |
||
---|---|---|---|---|
European | British | American | ||
Leaded tin bronze | CuSn11Pb2-C / CuSn11Pb2-B | CC482K / CB482K (EN 1982) | PB4 (BS 1400) | C92700 (ASTM B 505) |
Other name: Def Stan 02 838 Part 1, NES 838 Part 1, SAE 65c, NES 838, C90710 (AS 1565:1985), 904D (AS 1565:1974)
The equivalence between the standards is not absolute and some variations in composition can exist.
Chemical Composition in %, (EN 1982:2017, Castings)
Cu | Sn | Pb | Zn | Ni | Al | Fe | Mn | P | S | Si | Sb | As | Cr | Bi | Cd | Se | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Min | 83.5 | 10.5 | 0.7 | - | - | - | - | - | - | - | - | - | - | - | - | - | - |
Max | 87.0 | 12.5 | 2.5 | 2.0 | 2.0 | 0.01 | 0.20 | 0.2 | 0.4 | 0.08 | 0.01 | 0.2 | - | - | - | - | - |
Chemical Composition in %, (EN 1982:2017, Ingots)
Cu | Sn | Pb | Zn | Ni | Al | Fe | Mn | P | S | Si | Sb | As | Cr | Bi | Cd | Se | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Min | 83.5 | 10.7 | 0.7 | - | - | - | - | - | - | - | - | - | - | - | - | - | - |
Max | 86.5 | 12.5 | 2.5 | 2.0 | 2.0 | 0.01 | 0.15 | 0.2 | 0.05 | 0.08 | 0.01 | 0.20 | - | - | - | - | - |
Mechanical Properties (EN 1982:2017, Continuous castings)
Rm | Tensile strength min. | 280 N/mm2 |
Rp0.2 | Proof Strength min. | 150 N/mm2 |
A | Elongation min. | 5 % |
HB | Brinell hardness min. | 90 HBW |
Properties:
- material combines high mechanical strength with good ductility, corrosion resistance and wear resistance
Application:
- industrial Restaurant Equipment,
- bearings for heavy loads and relatively low speeds,
- bearings,
- gear boxes,
- speed reducers,
- valve bodies,
- worm gears